MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Description

POLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and cast films with 4 mil and greater thickness. POLYBATCH® AC-20531L is recommended for protecting the contents of packaging and for extending the lifetime of the packaging film or container. This product does perform by migration to the surface of the film or container and therefore, could adversely affect heat sealing or printing if excessive amounts are used. POLYBATCH® AC-20531L has a slight yellow-green tint.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Moisture Absorption <= 0.100 %<= 0.100 %190°C; ASTM D789
Additive Loading 20 %20 %
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Descriptive Properties
Pellet Count 70pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate
Overview of materials for Polypropylene, Extrusion Grade
Aclo Accucomp Polyethylene LD0109L Low Density
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
Aclo Accucomp Polyethylene LD0102L Low Density

PASHU362 / 25326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.