AISI 5132H Steel
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 5000 Series Steel
;
Low Alloy Steel
;
Carbon Steel
;
Medium Carbon Steel
Key Words:
JIS SCr 3 H (Japan.), B.S. 530 A 36, B.S.530 H 36, B.S. Type 3, UNS H51320, ASTM A304, SAE J1268, DIN 1.7034, AFNOR 38 C 4 (Fr), UNI 38 Cr 4 KB (Ital.)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
7.85
g/cc
0.284
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
174 - 212
174 - 212
annealed and cold drawn.
Hardness, Knoop
215
215
Converted from Brinell
Hardness, Rockwell B
91
91
Converted from Brinell
Hardness, Rockwell C
12
12
Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers
202
202
Converted from Brinell
Modulus of Elasticity
205
GPa
29700
ksi
Typical for steel
Bulk Modulus
160
GPa
23200
ksi
Typical for steel.
Poissons Ratio
0.29
0.29
Calculated
Machinability
70 %
70 %
annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus
80.0
GPa
11600
ksi
Typical for steel
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.0000210
ohm-cm
@Temperature 20.0 °C
0.0000210
ohm-cm
@Temperature 68.0 °F
hardened and tempered specimen; unknown specimen
0.0000259
ohm-cm
@Temperature 100 °C
0.0000259
ohm-cm
@Temperature 212 °F
hardened and tempered specimen; unknown specimen
0.0000330
ohm-cm
@Temperature 200 °C
0.0000330
ohm-cm
@Temperature 392 °F
hardened and tempered specimen; unknown specimen
0.0000517
ohm-cm
@Temperature 400 °C
0.0000517
ohm-cm
@Temperature 752 °F
hardened and tempered specimen; unknown specimen
0.0000778
ohm-cm
@Temperature 600 °C
0.0000778
ohm-cm
@Temperature 1110 °F
hardened and tempered specimen; unknown specimen
0.0000934
ohm-cm
@Temperature 700 °C
0.0000934
ohm-cm
@Temperature 1290 °F
hardened and tempered specimen; unknown specimen
0.0001106
ohm-cm
@Temperature 800 °C
0.0001106
ohm-cm
@Temperature 1470 °F
hardened and tempered specimen; unknown specimen
0.0001145
ohm-cm
@Temperature 900 °C
0.0001145
ohm-cm
@Temperature 1650 °F
hardened and tempered specimen; unknown specimen
0.0001177
ohm-cm
@Temperature 1000 °C
0.0001177
ohm-cm
@Temperature 1830 °F
hardened and tempered specimen; unknown specimen
0.0001205
ohm-cm
@Temperature 1100 °C
0.0001205
ohm-cm
@Temperature 2010 °F
hardened and tempered specimen; unknown specimen
0.000123
ohm-cm
@Temperature 1200 °C
0.000123
ohm-cm
@Temperature 2190 °F
hardened and tempered specimen; unknown specimen
0.0001251
ohm-cm
@Temperature 1300 °C
0.0001251
ohm-cm
@Temperature 2370 °F
hardened and tempered specimen; unknown specimen
Thermal Properties
Metric
English
Comments
Specific Heat Capacity
0.494
J/g-°C
@Temperature >=100 °C
0.118
BTU/lb-°F
@Temperature >=212 °F
annealed.
0.502
J/g-°C
@Temperature 150 - 200 °C
0.120
BTU/lb-°F
@Temperature 302 - 392 °F
Thermal Conductivity
44.3
W/m-K
@Temperature 200 °C
307
BTU-in/hr-ft²-°F
@Temperature 392 °F
Tested when annealed.
46.5
W/m-K
@Temperature 100 °C
323
BTU-in/hr-ft²-°F
@Temperature 212 °F
Tested when annealed.
48.6
W/m-K
@Temperature 0.000 °C
337
BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Tested when annealed.
Component Elements Properties
Metric
English
Comments
Carbon, C
0.29 - 0.35 %
0.29 - 0.35 %
Chromium, Cr
0.65 - 1.1 %
0.65 - 1.1 %
Iron, Fe
97.275 - 98.41 %
97.275 - 98.41 %
As remainder
Manganese, Mn
0.50 - 0.90 %
0.50 - 0.90 %
Phosphorus, P
<= 0.035 %
<= 0.035 %
Silicon, Si
0.15 - 0.30 %
0.15 - 0.30 %
Sulfur, S
<= 0.040 %
<= 0.040 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AISI 5135 Steel
AISI 5135H Steel
AISI 5132 Steel
AISI 4037H Steel
AISI 5130 Steel
M513BB / 8062
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.