Key features: High Transparency Common Uses: Humidifiers, optical instruments.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension. Data provided by Korea Kumho Petrochemical Co., Ltd. |