Orevac® OE807 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers. Orevac® OE807 is characterized by a high level of maleic anhydride. Information provided by Arkema Group |