MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Abatron AboCast 8101-5/AboCure 8101-5 5-Minute Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboCast 8101-5/AboCure 8101-5 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is a thixotropic (Vaseline-like consistency) form of the 8012-9 System. It is translucent, and clear in thin layers. It is used where 8012-9 would be too runny. It does not have the brittleness typical of conventional 5-minute epoxies. It also provides high resistance to weather, water, salt spray, alkalis, diluted acids, several fuels, solvents, and other chemicals. Unlike other epoxies, a thin layer of this compound does not need any longer to harden than a thick casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  13
@Time 601 sec
13
@Time 0.167 hour
 33
@Time 1800 sec
33
@Time 0.500 hour
 60
@Time 3600 sec
60
@Time 1.00 hour
 74
@Time 86400 sec
74
@Time 24.0 hour
Shear Strength 15.7 MPa2270 psiTensile lap
 
Processing PropertiesMetricEnglishComments
Pot Life 5.0 min5.0 min
Gel Time 5.00 min
@Thickness 1.27 mm
5.00 min
@Thickness 0.0500 in
 
Descriptive Properties
ColorTranslucent
Parts by Weight (pbw)100AboCast 8101-5
 100AboCure 8101-5
ViscosityVaseline-like

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Abatron AboWeld 8101-6/AboCure 8101-6 Epoxy
Abatron AboCast 10-5/AboCure 50-3 Epoxy
Sumitomo Bakelite DurezĀ® 33458 Phenolic Resin

PABC805 / 107789

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.