Weight per Epoxide (EEW, g/eq) 675 to 775. Max color is 1. Comments/Applications: "Type 2 1/2" epoxy resin with extremely good flow and very good powder stability. Data provided by Ciba Specialty Chemicals. Ciba Specialty Chemicals has been acquired by Huntsman. |