MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ductile Iron tension grade 65-45-12
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Carbon represents the total carbon in the listed composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 65-45-12 ductile iron is specified to have a minimum tensile strength of 65 ksi (448 MPa), a yield strength of 45 ksi (310 MPa) and an elongation of 12%. Determined for a single temperature of ductile iron, heat treated to approximate various standard grades. Properties were obtained using test bars machined from 25 mm keel blocks.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.10 - 7.20 g/cc0.257 - 0.260 lb/in³Typical value of ductile iron
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 167167
Hardness, Knoop 185185Converted from Brinell
Hardness, Vickers 173173Approximated. Converted from Brinell hardness.
Tensile Strength, Ultimate 464 MPa67300 psi
Tensile Strength, Yield 332 MPa
@Strain 0.2 %
48200 psi
@Strain 0.2 %
Elongation at Break 15 %15 %In 50 mm.
Modulus of Elasticity 168 GPa24400 ksi
Poissons Ratio 0.290.29
Shear Modulus 65.0 GPa9430 ksicalculated
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.0 - 3.8 %3.0 - 3.8 %
Cerium, Ce 0.0050 - 0.20 %0.0050 - 0.20 %
Chromium, Cr 0.030 - 0.070 %0.030 - 0.070 %
Copper, Cu 0.15 - 1.0 %0.15 - 1.0 %
Iron, Fe 90.738 - 94.175 %90.738 - 94.175 %
Magnesium, Mg 0.030 - 0.060 %0.030 - 0.060 %
Manganese, Mn 0.15 - 1.0 %0.15 - 1.0 %
Molybdenum, Mo 0.010 - 0.10 %0.010 - 0.10 %
Nickel, Ni 0.050 - 0.20 %0.050 - 0.20 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 1.8 - 2.8 %1.8 - 2.8 %
Sulfur, S <= 0.0020 %<= 0.0020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 65-45-12
Ductile Iron tension grade 60-40-18
Ductile Iron compression grade 65-45-12
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536
Ductile Iron grade 100-70-03

MDFE16 / 12013

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.