MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Multibase TPSiV® 3011-50A Thermoplastic Silicone Vulcanizate  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV); Polyurethane, TP; Silicone, Thermoplastic

Material Notes: TPV product based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.

Thermoplastic polyurethane based TPSiV™ (3010, 3011, 3111, 3040, 3340 grades) combine the benefits of excellent abrasion resistance from the polyurethane as well as the lower coefficient of friction and improved temperature properties from the silicone rubber.
TPSiV™ 3011-50A / 60A / 70A / 85A: General purpose grades designed for both injection molding and extrusion applications. Plasticizer free (except the 50A product), which results in excellent bonding via 2-shot molding or co-extrusion to PC, ABS, PU, and PVC. They display good tensile and tear strength.

Information provided by Multibase. Multibase is now a DuPont brand; this grade was discontinued prior to DuPont's acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 585810 sec; ASTM D2240
Tensile Strength at Break 11.0 MPa1600 psiASTM D412
Elongation at Break 680 %680 %ASTM D412
Tear Strength 40.3 kN/m230 pliASTM D412
Taber Abrasion, mg/1000 Cycles 6060ASTM D1044
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
 84 %
@Temperature 120 °C,
Time 79200 sec
84 %
@Temperature 248 °F,
Time 22.0 hour
Tensile Set 10 %10 %100%; ASTM D412
 34 %34 %3; ASTM D412
 60 %60 %At Break; ASTM D412
 60 %60 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 °C356 °F
Middle Barrel Temperature 190 °C374 °F
Front Barrel Temperature 200 °C392 °F
Nozzle Temperature 205 °C401 °F
Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 4 hour2 - 4 hour
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase TPSiV® 3010-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3010-50A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3011-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3040-85A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4200-50A Thermoplastic Silicone Vulcanizate

PMULTI304 / 93494

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.