MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.780 - 3.10 g/cc0.0282 - 0.112 lb/in³Average value: 0.921 g/cc Grade Count:538
Filler Content 10.0 - 30.0 %10.0 - 30.0 %Average value: 20.0 % Grade Count:4
Water Absorption 0.0100 - 0.0500 %0.0100 - 0.0500 %Average value: 0.0171 % Grade Count:21
Oxidative Induction Time (OIT) >= 35.0 min
@Temperature 210 - 210 °C
>= 35.0 min
@Temperature 410 - 410 °F
Average value: 35.0 min Grade Count:1
Maximum Moisture Content  0.200 - 0.250
@Temperature 120 - 120 °C
0.200 - 0.250
@Temperature 248 - 248 °F
Average value: 0.225 Grade Count:2
 0.200 - 0.250
@Time 299 - 299 sec
0.200 - 0.250
@Time 0.0830 - 0.0830 hour
Average value: 0.225 Grade Count:2
Thickness 50.0 - 840 microns1.97 - 33.1 milAverage value: 293 microns Grade Count:5
Linear Mold Shrinkage 0.00400 - 0.0252 cm/cm0.00400 - 0.0252 in/inAverage value: 0.0152 cm/cm Grade Count:89
Linear Mold Shrinkage, Transverse 0.00110 - 0.0263 cm/cm0.00110 - 0.0263 in/inAverage value: 0.0150 cm/cm Grade Count:24
Melt Flow 0.200 - 130 g/10 min0.200 - 130 g/10 minAverage value: 22.1 g/10 min Grade Count:616
Ash 2.00 - 24.0 %2.00 - 24.0 %Average value: 13.8 % Grade Count:3
 <= 2.00 %
@Temperature 600 - 600 °C
<= 2.00 %
@Temperature 1110 - 1110 °F
Average value: 2.00 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 49.0 - 11249.0 - 112Average value: 87.7 Grade Count:251
Hardness, Shore D 40.0 - 75.040.0 - 75.0Average value: 59.6 Grade Count:28
Ball Indentation Hardness 46.0 - 81.0 MPa6670 - 11700 psiAverage value: 58.2 MPa Grade Count:13
Tensile Strength, Ultimate 5.00 - 400 MPa725 - 58000 psiAverage value: 34.5 MPa Grade Count:78
Film Tensile Strength at Yield, MD 8.69 - 30.8 MPa1260 - 4470 psiAverage value: 16.9 MPa Grade Count:4
Film Tensile Strength at Yield, TD 9.03 - 25.2 MPa1310 - 3650 psiAverage value: 15.1 MPa Grade Count:3
Tensile Strength, Yield 5.50 - 300 MPa798 - 43500 psiAverage value: 25.7 MPa Grade Count:551
Film Elongation at Break, MD 380 - 1180 %380 - 1180 %Average value: 658 % Grade Count:10
Film Elongation at Break, TD 570 - 900 %570 - 900 %Average value: 760 % Grade Count:8
Elongation at Break 1.80 - 900 %1.80 - 900 %Average value: 167 % Grade Count:225
 5.00 - 11.0 %
@Temperature -17.7 - 90.0 °C
5.00 - 11.0 %
@Temperature 0.126 - 194 °F
Average value: 22.3 % Grade Count:11
Elongation at Yield 0.900 - 350 %0.900 - 350 %Average value: 9.15 % Grade Count:364
 8.50 - 9.00 %
@Temperature 60.0 - 90.0 °C
8.50 - 9.00 %
@Temperature 140 - 194 °F
Average value: 8.75 % Grade Count:1
Modulus of Elasticity 0.475 - 3.50 GPa68.9 - 508 ksiAverage value: 1.31 GPa Grade Count:144
 0.650 - 1.10 GPa
@Temperature 60.0 - 90.0 °C
94.3 - 160 ksi
@Temperature 140 - 194 °F
Average value: 0.875 GPa Grade Count:1
Flexural Yield Strength 17.0 - 48.3 MPa2470 - 7000 psiAverage value: 29.6 MPa Grade Count:35
Flexural Modulus 0.0850 - 11.5 GPa12.3 - 1670 ksiAverage value: 1.27 GPa Grade Count:533
Secant Modulus 0.827 - 1.34 GPa120 - 195 ksiAverage value: 1.10 GPa Grade Count:12
Secant Modulus, MD 0.150 - 0.896 GPa21.8 - 130 ksiAverage value: 0.373 GPa Grade Count:9
Secant Modulus, TD 0.166 - 0.772 GPa24.1 - 112 ksiAverage value: 0.393 GPa Grade Count:8
Izod Impact, Notched 0.0280 J/cm - NB0.0525 ft-lb/in - NBAverage value: 1.91 J/cm Grade Count:382
 0.0400 - 980.567 J/cm
@Temperature -40.0 - 3.89 °C
0.0749 - 1837.00 ft-lb/in
@Temperature -40.0 - 39.0 °F
Average value: 0.719 J/cm Grade Count:119
 0.850 - 0.850 J/cm
@Temperature -10.0 - 0.000 °C
1.59 - 1.59 ft-lb/in
@Temperature 14.0 - 32.0 °F
Average value: 0.719 J/cm Grade Count:2
 0.850 - 0.850 J/cm
@Thickness 3.17 - 6.40 mm
1.59 - 1.59 ft-lb/in
@Thickness 0.125 - 0.252 in
Average value: 0.719 J/cm Grade Count:2
 0.250 - 1.35 J/cm
@Diameter 0.125 - 3.17 mm
0.468 - 2.53 ft-lb/in
@Diameter 0.00492 - 0.125 in
Average value: 0.719 J/cm Grade Count:11
 0.250 - 1.35 J/cm
@Temperature -20.0 - -20.0 °C
0.468 - 2.53 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.719 J/cm Grade Count:11
Izod Impact, Unnotched 0.300 J/cm - NB0.562 ft-lb/in - NBAverage value: 3.20 J/cm Grade Count:70
 0.200 J/cm - NB
@Temperature -30.0 - 0.000 °C
0.375 ft-lb/in - NB
@Temperature -22.0 - 32.0 °F
Average value: 0.600 J/cm Grade Count:46
 1.0678 - 1.0678 J/cm
@Temperature -20.0 - -20.0 °C
2.0004 - 2.0004 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.600 J/cm Grade Count:1
 1.0678 - 1.0678 J/cm
@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 0.600 J/cm Grade Count:1
Izod Impact, Notched (ISO) 2.50 - 21000 kJ/m²1.19 - 9990 ft-lb/in²Average value: 25.1 kJ/m² Grade Count:97
 2.00 kJ/m² - NB
@Temperature -40.0 - 3.89 °C
0.952 ft-lb/in² - NB
@Temperature -40.0 - 39.0 °F
Average value: 6.65 kJ/m² Grade Count:64
Izod Impact, Unnotched (ISO) 6.00 - 6.00 kJ/m²
@Temperature -40.0 - -40.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 0.600 - 1000 J/cm²2.86 - 4760 ft-lb/in²Average value: 3.65 J/cm² Grade Count:20
 0.450 - 999.9 J/cm²
@Temperature -40.0 - -20.0 °C
2.14 - 4759 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 5.78 J/cm² Grade Count:14
Charpy Impact, Notched 0.130 - 1000 J/cm²0.619 - 4760 ft-lb/in²Average value: 2.66 J/cm² Grade Count:143
 0.100 - 12.0 J/cm²
@Temperature -40.0 - 0.000 °C
0.476 - 57.1 ft-lb/in²
@Temperature -40.0 - 32.0 °F
Average value: 0.896 J/cm² Grade Count:121
Gardner Impact 1.00 - 40.7 J0.738 - 30.0 ft-lbAverage value: 20.0 J Grade Count:57
 2.26422 - 40.6746 J
@Temperature -30.0 - 0.000 °C
1.67000 - 30.0000 ft-lb
@Temperature -22.0 - 32.0 °F
Average value: 23.9 J Grade Count:37
 16.6088 - 33.7825 J
@Temperature -30.0 - -28.9 °C
12.2500 - 24.9167 ft-lb
@Temperature -22.0 - -20.0 °F
Average value: 23.9 J Grade Count:15
 16.6088 - 33.7825 J
@Thickness 3.17 - 3.17 mm
12.2500 - 24.9167 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 23.9 J Grade Count:15
Dart Drop, Total Energy 40.6746 - 48.8095 J
@Temperature -29.0 - -29.0 °C
30.0000 - 36.0000 ft-lb
@Temperature -20.2 - -20.2 °F
Average value: 45.5 J Grade Count:3
Falling Dart Impact  5.09788 - 5.09788 J
@Temperature -30.0 - -30.0 °C
3.76000 - 3.76000 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 5.10 J Grade Count:1
 5.09788 - 5.09788 J
@Thickness 1.78 - 1.78 mm
3.76000 - 3.76000 ft-lb
@Thickness 0.0701 - 0.0701 in
Average value: 5.10 J Grade Count:1
Dart Drop Test 23.2 - 600 g0.0512 - 1.32 lbAverage value: 218 g Grade Count:5
Film Tensile Strength at Break, MD 17.9 - 72.4 MPa2600 - 10500 psiAverage value: 44.4 MPa Grade Count:9
Film Tensile Strength at Break, TD 20.6 - 60.0 MPa2990 - 8700 psiAverage value: 32.0 MPa Grade Count:8
Tangent Modulus 740 - 1590 MPa107000 - 230000 psiAverage value: 1250 MPa Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+16 ohm-cm100 - 1.00e+16 ohm-cmAverage value: 3.55e+15 ohm-cm Grade Count:11
Surface Resistance 10000 - 1.00e+15 ohm10000 - 1.00e+15 ohmAverage value: 2.50e+14 ohm Grade Count:4
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 - 222 °C228 - 432 °FAverage value: 158 °C Grade Count:102
Crystallization Temperature 110 - 261 °C230 - 502 °FAverage value: 193 °C Grade Count:16
Maximum Service Temperature, Air 110 - 150 °C230 - 302 °FAverage value: 122 °C Grade Count:5
Hot Ball Pressure Test 115 - 125 °C239 - 257 °FAverage value: 122 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 45.6 - 150 °C114 - 302 °FAverage value: 97.4 °C Grade Count:495
Deflection Temperature at 1.8 MPa (264 psi) 37.8 - 115 °C100 - 239 °FAverage value: 56.1 °C Grade Count:123
 105 - 105 °C
@Temperature 0.250 - 0.250 °C
221 - 221 °F
@Temperature 32.5 - 32.5 °F
Average value: 105 °C Grade Count:1
Vicat Softening Point 50.0 - 155 °C122 - 311 °FAverage value: 133 °C Grade Count:153
Brittleness Temperature -60.0 - 0.000 °C-76.0 - 32.0 °FAverage value: -44.8 °C Grade Count:16
Flammability, UL94 HB - V-0HB - V-0Grade Count:50
Flash Point 340 °C644 °FAverage value: 340 °C Grade Count:8
Oxygen Index 21.0 - 29.0 %21.0 - 29.0 %Average value: 24.1 % Grade Count:8
Glow Wire Test 550 - 750 °C1020 - 1380 °FAverage value: 664 °C Grade Count:6
Ignition Temperature 350 °C662 °FAverage value: 350 °C Grade Count:7
 
Optical PropertiesMetricEnglishComments
Haze 4.00 - 60.0 %4.00 - 60.0 %Average value: 18.3 % Grade Count:23
Gloss 3.00 - 97.0 %3.00 - 97.0 %Average value: 56.7 % Grade Count:20
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 274 °C356 - 525 °FAverage value: 219 °C Grade Count:63
Nozzle Temperature 182 - 243 °C360 - 470 °FAverage value: 214 °C Grade Count:16
Melt Temperature 120 - 270 °C248 - 518 °FAverage value: 227 °C Grade Count:103
Head Temperature 210 °C410 °FAverage value: 210 °C Grade Count:3
Mold Temperature 15.0 - 80.0 °C59.0 - 176 °FAverage value: 42.9 °C Grade Count:75
Drying Temperature 70.0 - 100 °C158 - 212 °FAverage value: 84.0 °C Grade Count:33
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.138 % Grade Count:4
Injection Pressure 2.76 - 140 MPa400 - 20300 psiAverage value: 72.8 MPa Grade Count:18
Cure Time 0.0250 - 0.0417 min0.000417 - 0.000694 hourAverage value: 0.0333 min Grade Count:32

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler

O4702 / 78372

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.