Marex Composites Mycell M080 PVC Foam Core
Categories:
Other Engineering Material
;
Composite Core Material
;
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Foam Grade
Material Notes:
Mycell is a PVC structural foam material that Marex Composites customizes for standard finishes from Maricell in Italy.
Property data reported are nominal/average values.
Information provided by Marex Composites.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.0800
g/cc
0.00289
lb/in³
ISO 845
Water Absorption
1.0 %
1.0 %
Mechanical Properties
Metric
English
Comments
Tensile Strength
1.92
MPa
278
psi
ASTM D1623
Elongation at Break
30 %
30 %
Shear elongation; ISO 1922
Tensile Modulus
0.0870
GPa
12.6
ksi
ASTM D1623
Compressive Strength
1.36
MPa
197
psi
ISO 844
Compressive Modulus
0.0920
GPa
13.3
ksi
ISO 844
Shear Modulus
0.0280
GPa
4.06
ksi
ASTM C393
Shear Strength
1.37
MPa
199
psi
ASTM C393
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.0330
W/m-K
0.229
BTU-in/hr-ft²-°F
ISO 8301
Descriptive Properties
Color
Green
Fire Resistance
DIN5510 S4 SR2 ST2 FED<1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for PVC, Foam Grade
Karina KAPU 8035/1-Y Ivory PVC Compound
DIAB Klegecell® R 75 Rigid, Closed Cell PVC Foam Core Material
CoreLite PVC 80 Closed-Cell PVC Foam Sheet
PMAREX973 / 230569
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.