MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 3004-H36
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A93004; ISO AlMn1Mg1; Aluminium 3004-H36; AA3004-H36; Al3004-H36
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 9393Converted from Brinell Hardness Value
Hardness, Vickers 8080Converted from Brinell Hardness Value
Tensile Strength, Ultimate 262 MPa38000 psiAA; Typical
 240 - 285 MPa
@Thickness 0.152 - 4.11 mm
34800 - 41300 psi
@Thickness 0.00600 - 0.162 in
Tensile Strength, Yield 228 MPa33000 psiAA; Typical
 >= 195 MPa
@Thickness 0.152 - 4.11 mm
>= 28300 psi
@Thickness 0.00600 - 0.162 in
Elongation at Break  1.0 - 4.0 %
@Thickness 0.152 - 4.11 mm
1.0 - 4.0 %
@Thickness 0.00600 - 0.162 in
 5.0 %
@Thickness 1.59 mm
5.0 %
@Thickness 0.0625 in
AA; Typical
 9.0 %
@Diameter 12.7 mm
9.0 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 68.9 GPa10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.350.35
Fatigue Strength 110 MPa
@# of Cycles 5.00e+8
16000 psi
@# of Cycles 5.00e+8
completely reversed stress; RR Moore machine/specimen
Shear Modulus 25.0 GPa3630 ksi
Shear Strength 138 MPa20000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000416 ohm-cm
@Temperature 20.0 °C
0.00000416 ohm-cm
@Temperature 68.0 °F
AA; Typical
Magnetic Susceptibility 8.0e-78.0e-7cgs/g at 25ºC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.5 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.9 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.2 µm/m-°C
@Temperature 20.0 - 100 °C
12.9 µin/in-°F
@Temperature 68.0 - 212 °F
 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
13.3 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.1 µm/m-°C
@Temperature 20.0 - 200 °C
13.4 µin/in-°F
@Temperature 68.0 - 392 °F
 25.1 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.893 J/g-°C0.213 BTU/lb-°F
Thermal Conductivity 163 W/m-K1130 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 629.4 - 654 °C1165 - 1210 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 629.4 °C1165 °FAA; Typical
Liquidus 654 °C1210 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.5 - 98.2 %95.5 - 98.2 %As remainder
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.80 - 1.3 %0.80 - 1.3 %
Manganese, Mn 1.0 - 1.5 %1.0 - 1.5 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 3004-H32
Aluminum 3004-H38
Aluminum 3004-H34
Aluminum 3004-H19
Aluminum 3004-O

MA3004H36 / 8995

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.