MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Buckeye Polymers BP RPP 2012 T BLK Polypropylene, Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.

    Product Features:
  • Increased stiffness and heat deflection
  • Good UV resistance
  • Industrial, appliance, construction markets
  • Good scratch and mar resistance
  • Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 - 1.09 g/cc1.02 - 1.09 g/ccASTM D792
Melt Flow 6.0 - 15 g/10 min6.0 - 15 g/10 minASTM D1238
Ash 18 - 23 %18 - 23 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 26.0 MPa>= 3770 psiASTM D638
Flexural Modulus >= 1.62458 GPa>= 235.625 ksiASTM D790
Izod Impact, Notched >= 0.198 J/cm>= 0.370 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 4008 TR BLK Polypropylene, Talc Filled
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled
LyondellBasell Hifax HKC 426P BLACK Polypropylene with 20% Talc Filler
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded
Mytex Polymers AS65KW-1ATM Polypropylene, Talc filled, Compounded

PBUCK031 / 104498

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.