MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo Plexiglas® Diffuse™ V045-68209 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Plexiglas® Diffuse™ V045-68209 is a thermoplastic acrylic resin sufficiently concentrated to be used in blend formulations via extrusion to tailor lens properties in the LED lighting market. It is characterized by its exceptional hiding performance and high light transmission.

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 0.3 %0.3 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.002 - 0.006 cm/cm0.002 - 0.006 in/inASTM D955
Melt Flow 1.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.7 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8686ASTM D785
Tensile Strength, Ultimate 60.7 MPa8800 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 2.90 GPa420 ksiASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiASTM D790
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °Fannealed; ASTM D648
Vicat Softening Point 104 °C219 °F50°C/hr; 50N; ASTM D1525
 109 °C228 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze >= 100 %
@Thickness 2.03 mm
>= 100 %
@Thickness 0.0800 in
ASTM D1003
Transmission, Visible 79 %
@Thickness 2.03 mm
79 %
@Thickness 0.0800 in
ASTM D1003
 
Descriptive Properties
ASTM ClassificationPMMA 0111T0V1ASTM D788

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® Diffuse™ DR®-66151 Acrylic Resin
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Trinseo Solarkote™ A200 Acrylic
Chi Mei Acryrex® CM-205 PMMA

PARKG043m / 191487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.