Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well suited for deep drawing and bending. Applications: Used in a variety of interior applications where material cost and corrosion performance are important factors. Typical applications include: - Washing machines
- Dish-washers
- Sinks
- Electrical tie-wire
- Vine wire
- Sink rims
- Counter tops
- Cooker hoods
- Refrigerators
- Tableware
- Restaurant equipment
- Indoor cladding
- Flue-gas ducts
Available in cold rolled narrow strip, bar, and rod forms. |
EN 1.4016; ASTM 430; JIS SUS 430 |