Product Characteristics- Easy filling of thin-walled parts
- Exceptional mold release
- Improved cycle times in hard to fill parts
- Food Contact Compliant
- UL Classification 94HB
- USP Class VI
Typical Applications - Color concentrate carrier
- Consumer containers, vials, jars, etc.
- Disposable cutlery
- Injection molded drink cups
Information provided by AmericasStyrenics LLC. |