MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact strength.

Regulatory Status: NA967000 meets the requirements of the Food and Drug Administration, 21 CFR 177.1520. This regulation allows the use of this olefin polymer "...in articles or components of articles intended for use in contact with food," except in cooking applications. Specific limitations or conditions of use do apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing NA967000 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil
Melt Flow 1.5 g/10 min1.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151molding; ASTM D2240
Tensile Strength at Break 10.3 MPa1500 psimolding; ASTM D638
Film Elongation at Break, MD 220 %220 %ASTM D882
Film Elongation at Break, TD 520 %520 %ASTM D882
Elongation at Break 600 %600 %molding; ASTM D638
Elmendorf Tear Strength MD 390 g390 gASTM D1922
Elmendorf Tear Strength TD 100 g100 gASTM D1922
Dart Drop 4.72 g/micron120 g/milF50; ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa3600 psiASTM D882
Film Tensile Strength at Break, TD 17.9 MPa2600 psiASTM D882
1% Secant Modulus, MD 179 MPa26000 psiASTM D882
1% Secant Modulus, TD 228 MPa33000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °Fmolding; ASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °Fmolding; ASTM D746
 0.500 °C32.9 °Fmolding, notched; ASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 °C350 °F
Die Opening 0.0635 cm0.0250 in
Blow-up Ratio (BUR) 2.02.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene
BP Amoco ACCPRO® 9119X Extrusion Grade Polypropylene
Ineos H00M-01 Polypropylene Homopolymer
Ineos H03G-03 Polypropylene Homopolymer

PEQU0830 / 104186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.