MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sylvania SD252 Tungsten & Chrome Based Thermal Spray Powder
Categories: Ceramic; Carbide; Metal; Nonferrous Metal; Tungsten Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SD252 is plasma densified tungsten carbide-cobalt spray powder, designed for use as a wear resistant coating. The major constituent is W2C. There is also some WC, as well as complex Co-W-C compounds. Its flow characteristics are excellent and the apparent density is high.

Applications

  • Thread Guides
  • Screw Conveyors
  • Jet-engine Components
  • Pump Parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 6.00 - 6.40 g/cc0.217 - 0.231 lb/in³
Particle Size <= 31 µm<= 31 µm4 wt% max; ASTM B822
 <= 62 µm<= 62 µm43 wt% max; ASTM B822
 <= 176 µm<= 176 µm100 wt% min; ASTM B822
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.6 - 4.2 %3.6 - 4.2 %
Cobalt, Co 11 - 13 %11 - 13 %
Iron, Fe <= 2.0 %<= 2.0 %
Tungsten, W >= 81 %>= 81 %
 
Descriptive Properties
Hall Flow, seconds/50g15ASTM B213

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, W2C
CoorsTek Tungsten Carbide, WC
Tungsten Carbide, WC
Tungsten, W
American Elements Tungsten Carbide Nanoparticles

CSYLV13 / 2312

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.