MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Adsyl 7623 XCP Polyolefin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade (Polyolefin)

Material Notes: Adsyl resins are propylene plus ethylene and butene based random copolymers and terpolymers with high comonomer ratios that deliver improved sealing properties. Grades of Adsyl resins can be used in all of the main film extrusion technologies, such as BOPP, Double Bubble, Cast and Blown Film. Adsyl grades are mainly used for skin layers in co-extruded or coated film structures to provide sealing functionality.

Adsyl 7623 XCP is an advanced polyolefin, specially designed for use as a sealing or metalized layer in co-extruded film applications. This grade features a very low seal initiation temperature. It contains anti-block additives. Applications: Food Packaging Film, Lamination Film, Shrink Film, Stationery Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method A; ISO 1183
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.0 MPa
@Thickness 0.0500 mm
2030 psi
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-1,-3
Film Tensile Strength at Yield, TD 14.0 MPa
@Thickness 0.0500 mm
2030 psi
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-1,-3
Film Elongation at Break, MD 900 %
@Thickness 0.0500 mm
900 %
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Break, TD 800 %
@Thickness 0.0500 mm
800 %
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Yield, MD 17 %
@Thickness 0.0500 mm
17 %
@Thickness 0.00197 in
500 mm/min, cast film; ISO 527-3
Film Elongation at Yield, TD 15 %
@Thickness 0.0500 mm
15 %
@Thickness 0.00197 in
500 mm/min, cast film; ISO 527-3
Secant Modulus, MD 0.280 GPa
@Thickness 0.0500 mm
40.6 ksi
@Thickness 0.00197 in
23 mm/min, cast film; ISO 527-1,-3
Secant Modulus, TD 0.280 GPa
@Thickness 0.0500 mm
40.6 ksi
@Thickness 0.00197 in
23 mm/min, cast film; ISO 527-1,-3
Film Tensile Strength at Break, MD 45.0 MPa
@Thickness 0.0500 mm
6530 psi
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-3
Film Tensile Strength at Break, TD 35.0 MPa
@Thickness 0.0500 mm
5080 psi
@Thickness 0.00197 in
500 mm/min, Cast Film; ISO 527-3
Heat Seal Strength Initiation Temperature 105 °C221 °FLYB method
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C144 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 107 °C225 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 1.2 %
@Thickness 0.0500 mm
1.2 %
@Thickness 0.00197 in
ASTM D 1003
Gloss 87 %
@Thickness 0.0500 mm
87 %
@Thickness 0.00197 in
45°; ASTM D 2457
 
Descriptive Properties
Processing MethodBOPP, Cast Film, Double Bubble

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT7046 / 218685

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.