MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BJB Enterprises F-180 REV 1 A/B Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: The F-1 Series addresses the need for shorter processing times and higher part production. These products exhibit excellent physical properties and easily process at room temperature. The easy mix ratio is convenient and cartridge dispense friendly. For longer work times consider the M Series or L Series of elastomers.

Features: RoHS/REACH Compliant, Popular for Parts & Molds, High Tensile & Tear Strength, Special Effects & Props, Over Molding, Easy to Pigment.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  1.067 g/cc
@Temperature 25.0 °C
1.067 g/cc
@Temperature 77.0 °F
Part A
 1.09 g/cc
@Temperature 25.0 °C
1.09 g/cc
@Temperature 77.0 °F
Part B
Density 1.10 g/cc0.0397 lb/in³7 day ambient cure; ASTM D792-00
 1.10 g/cc0.0397 lb/in³Elevated temp cure; ASTM D792-00
Brookfield Viscosity  685 cP
@Temperature 25.0 °C
685 cP
@Temperature 77.0 °F
Part B
 2600 cP
@Temperature 25.0 °C
2600 cP
@Temperature 77.0 °F
Mixed Part A & Part B
 4450 cP
@Temperature 25.0 °C
4450 cP
@Temperature 77.0 °F
Part A
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in1" depth.; ASTM D2566
Storage Temperature 18.3 - 26.7 °C65.0 - 80.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8575 - 857 day ambient cure; ASTM D2240-04e1
 75 - 8575 - 85Elevated temp cure; ASTM D2240-04e1
Tensile Strength 25.6 MPa3720 psiElevated temp cure; ASTM D412-98a(2002)e1
Elongation at Break 650 %650 %Elevated temp cure; ASTM D638-03
Tensile Modulus 0.0145 GPa2.10 ksiElevated temp cure; ASTM D412-98a(2002)e1
Tear Strength 67.5 kN/m385 pliElevated temp cure; ASTM D624-00e1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  5.285
@Frequency 1e+6 Hz
5.285
@Frequency 1e+6 Hz
7 day ambient cure; ASTM D150-87
 5.285
@Frequency 1e+6 Hz
5.285
@Frequency 1e+6 Hz
Elevated temp cure; ASTM D150-87
Dissipation Factor  0.0671
@Frequency 1e+6 Hz
0.0671
@Frequency 1e+6 Hz
7 day ambient cure; ASTM D150-87
 0.0671
@Frequency 1e+6 Hz
0.0671
@Frequency 1e+6 Hz
Elevated temp cure; ASTM D150-87
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 93.3 °C<= 200 °FMax cure temp.
Cure Time  60.0 - 180 min
@Temperature 25.0 °C
1.00 - 3.00 hour
@Temperature 77.0 °F
Step 1 recommended high temp cure (as tested).
 960 min
@Temperature 71.1 °C
16.0 hour
@Temperature 160 °F
Step 2 recommended high temp cure (as tested).
 7200 - 10100 min
@Temperature 25.0 °C
120 - 168 hour
@Temperature 77.0 °F
Optional low temp cure
Working Life 8.00 - 9.00 min
@Temperature 25.0 °C
8.00 - 9.00 min
@Temperature 77.0 °F
100 g.
Gel Time 11.0 - 12.0 min11.0 - 12.0 min
Shelf Life 6.00 Month6.00 MonthStored at recommended temperatures. Purge opened containers with dry nitrogen before resealing.
 
Descriptive Properties
Color / AppearanceAmberPart B
 Pale YellowPart A
 Translucent Amber7 day ambient cure
 Translucent AmberElevated temp cure
Demold Time (hrs)2 - 3@ 77°F
Mix Ratio by volume100 to 49Part A to Part B. (cartridge dispense friendly)
Mix Ratio by weight100 to 50Part A to Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBJB9919 / 287699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.