MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI 1010 Steel, cold drawn
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Used widely in low strength applications. Good formability, fair machinability, can be hardened by cyaniding. Suitable for magnet core applications

Key Words: UNS G10100, AISI1010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 105105
Hardness, Knoop 123123Converted from Brinell
Hardness, Rockwell B 6060Converted from Brinell
Hardness, Vickers 108108Converted from Brinell
Tensile Strength, Ultimate 365 MPa52900 psi
Tensile Strength, Yield 305 MPa44200 psi
Elongation at Break 20 %20 %In 50 mm
Reduction of Area 40 %40 %
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Machinability 55 %55 %Based on AISI 1212 steel = 100%. Group I bar, rod, and wire products machinability can be improved by cold drawing.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000143 ohm-cm0.0000143 ohm-cmcondition unknown
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.2 µm/m-°C
@Temperature 0.000 - 100 °C
6.78 µin/in-°F
@Temperature 32.0 - 212 °F
 13.5 µm/m-°C
@Temperature 0.000 - 300 °C
7.50 µin/in-°F
@Temperature 32.0 - 572 °F
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
7.89 µin/in-°F
@Temperature 32.0 - 932 °F
Specific Heat Capacity  0.448 J/g-°C
@Temperature >=100 °C
0.107 BTU/lb-°F
@Temperature >=212 °F
condition unknown
 0.498 J/g-°C
@Temperature 150 - 200 °C
0.119 BTU/lb-°F
@Temperature 302 - 392 °F
 0.519 J/g-°C
@Temperature 200 - 250 °C
0.124 BTU/lb-°F
@Temperature 392 - 482 °F
 0.536 J/g-°C
@Temperature 250 - 300 °C
0.128 BTU/lb-°F
@Temperature 482 - 572 °F
 0.565 J/g-°C
@Temperature 300 - 350 °C
0.135 BTU/lb-°F
@Temperature 572 - 662 °F
 0.590 J/g-°C
@Temperature 350 - 400 °C
0.141 BTU/lb-°F
@Temperature 662 - 752 °F
 0.649 J/g-°C
@Temperature 400 - 450 °C
0.155 BTU/lb-°F
@Temperature 752 - 842 °F
 0.729 J/g-°C
@Temperature 550 - 600 °C
0.174 BTU/lb-°F
@Temperature 1020 - 1110 °F
 0.825 J/g-°C
@Temperature 650 - 700 °C
0.197 BTU/lb-°F
@Temperature 1200 - 1290 °F
Thermal Conductivity 49.8 W/m-K346 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.080 - 0.13 %0.080 - 0.13 %
Iron, Fe 99.18 - 99.62 %99.18 - 99.62 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1020 Steel, cold rolled
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
ASTM A500 Steel, grade A, shaped structural tubing
ASTM A500 Steel, grade B, shaped structural tubing

M1010A / 6782

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.