Highly Recyclable Nylon 12 Laser Sintering Material. Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates from 15 to 25%. Good temperature control is required to process this material. Information provided by Advanced Laser Materials (ALM). |