MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Goodfellow Iron 81/Boron 13.5/Silicon 3.5 Alloy
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal; Superalloy; Iron Base

Material Notes: Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.32 g/cc0.264 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 880880kg(f)/mm²
Tensile Strength at Break >= 700 MPa>= 102000 psi
Tensile Modulus 58.0 GPa8410 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000135 ohm-cm0.000135 ohm-cm
Magnetic Coercive Force, Hc 0.080 Oe0.080 Oe
Magnetic Saturation Flux Density, Bmax 16000 Gauss16000 Gauss
Magnetic Remanence, Br 0.70 Gauss0.70 GaussRemanence Ratio, Br/Bs
Curie Temperature 370 °C698 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 480 °C896 °F
Maximum Service Temperature, Air 125 °C257 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 13.5 %13.5 %
Carbon, C 2.0 %2.0 %
Iron, Fe 81 %81 %
Silicon, Si 3.5 %3.5 %
 
Descriptive Properties
Saturation magnetostriction (x10^-6)30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Less Common Metals Nd-Fe-B Cast Neodymium Iron Boron Alloy
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
Goodfellow Iron 79/Boron 16/Silicon 5 Alloy
Goodfellow Iron 78/Boron 13/Silicon 9 Alloy
Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy

NGOODF154 / 16226

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.