MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco TEGRA® ISO 220 Synthetic Compressor Oil HC
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Features

Chevron Tegra Synthetic Compressor Oil HC is a synthetic compressor lubricant. It is formulated to meet the demands of reciprocating compressors for gases other than air.

It is formulated with the highest quality polyalphaolefin (PAO) base fluids. PAO has inherent properties, such as excellent thermal and oxidative stability, high viscosity index, high flash and fire points, natural friction reducing ability, and excellent low temperature fluidity, which make Chevron Tegra Synthetic Compressor Oil HC especially well suited for the lubrication of compressor cylinders.

The ashless nature of Chevron Tegra Synthetic Compressor Oil HC makes it nonpoisonous to catalysts. The purity and thermal stability of this lubricant will substantially reduce the formation of sludge, deposits and sticky residues on compressor discharge valves, piping, and aftercooler tubing.

Applications

Chevron Tegra Synthetic Compressor Oil HC is designed to meet the needs of cylinder lubrication in reciprocating compressors for inert gases (e.g. nitrogen, hydrogen, carbon dioxide, etc.) or for hydrocarbon gases (e.g. ethylene, propylene, propane, butane, etc.).

The synthetic properties of Chevron Tegra Synthetic Compressor Oil HC reduce the problems associated with dilution by liquid hydrocarbons and by gas absorption at high pressures.

Chevron Tegra Synthetic Compressor Oil HC meets U.S. Food and Drug Administration (FDA) requirements, 21 CFR 178.3570, and is suitable for lubrication of ethylene and propylene compressors involved in the manufacture of polymeric food packaging.

Key Words: CPS Number: 259134; MSDS Number: 8269
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 36.7 °36.7 °
Viscosity Measurement 160160Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1077 SUS1077 SUS
Saybolt Viscosity at 210°F 129.7 SUS129.7 SUS
Kinematic Viscosity at 40°C (104°F) 209 cSt209 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 26.4 cSt26.4 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -51.0 °C-59.8 °FASTM D97
Flash Point 232 °C450 °FASTM D92
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Rubatex R4281 Flame Retardant Neoprene/EPDM/SBR Rubber Foam Sheet
Rubatex R4261 Flame Retardant Neoprene/EPDM/SBR Rubber Foam Sheet
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer
Ethylene Propylene Rubber (EPM, EPDM)

WCHEV367 / 74982

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.