MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plenco 4485 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is available in black, brown, and red.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³ASTM D1895
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Water Absorption 0.212 %0.212 %ASTM D570
Linear Mold Shrinkage 0.0081 cm/cm0.0081 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8484ASTM D785
Tensile Strength, Ultimate 55.0 MPa7980 psiASTM D638
Elongation at Break 0.82 %0.82 %ASTM D638
Tensile Modulus 8.10 GPa1170 ksiASTM D638
Flexural Strength 84.0 MPa12200 psiASTM D790
Flexural Modulus 7.50 GPa1090 ksiASTM D790
Compressive Strength 195 MPa28300 psiASTM D695
Poissons Ratio 0.350.35ASTM D638
Shear Modulus 3.00 GPa435 ksiCalculated
Izod Impact, Notched 0.151 J/cm0.283 ft-lb/inASTM D256
Charpy Impact, Notched 0.172 J/cm²0.819 ft-lb/in²ASTM D256
Impact 9696J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.90e+11 ohm-cm1.90e+11 ohm-cmASTM D247
Dielectric Constant 5.35.3ASTM D150
Dielectric Strength 10.0 kV/mm254 kV/inShort Time; ASTM D149
Dissipation Factor 0.0560.056ASTM D150
Arc Resistance 150 sec150 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 40.0 - 130 °C
27.8 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 203 °C397 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 166 °C331 °FASTM D648
Flammability, UL94 V-1
@Thickness 3.00 mm
V-1
@Thickness 0.118 in
Oxygen Index 31 %31 %ASTM D2863
Shrinkage 0.29 %0.29 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2308 Phenolic, Granular, Transfer Molded
Plenco 2308 Phenolic, Granular, Injection Molded
Plenco 2369 Phenolic, Granular, Compression Molded
Plenco 2311 Phenolic, Granular, Transfer Molded
Plenco 2311 Phenolic, Granular, Injection Molded

PLEL88 / 50661

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.