MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Ketron™ Sterra™ CA30 PEEK Recycled poly-ether-ether-ketone
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: 30% carbon fiber-reinforced PEEK grade with recycled contents. The addition of carbon fibers enhances the compressive strength and stiffness of PEEK, and dramatically lowers its expansion rate.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Water Absorption at Saturation 0.300 %0.300 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ASTM D785
Hardness, Shore D 90.090.0ISO 868
Tensile Strength 144 MPa20900 psiISO 527-1/-2 (7)
Flexural Strength 220 MPa31900 psiISO 178 (12)
Compressive Yield Strength  69.0 MPa
@Strain 1.00 %
10000 psi
@Strain 1.00 %
ISO 604 (10)
 125 MPa
@Strain 2.00 %
18100 psi
@Strain 2.00 %
ISO 604 (10)
 170 MPa
@Strain 5.00 %
24700 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 103 MPa14900 psiASTM D732
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmANSI/ESD STM 11.11
Dielectric Strength 1.26 kV/mm32.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C10.0 µin/in-°FASTM E-831 (TMA)
 25.0 µm/m-°C
@Temperature 23.0 - 100 °C
13.9 µin/in-°F
@Temperature 73.4 - 212 °F
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
 55.0 µm/m-°C
@Temperature >=150 °C
30.6 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.920 W/m-K6.38 BTU-in/hr-ft²-°F
 0.922 W/m-K6.40 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 250 °C482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMU754 / 323871

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.