MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboTar 8607-1 Solventless Tar-Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboTar 8607-1 is a 2-part tar-epoxy lower cost system for filling and leveling pot holes and grossly uneven flooring. It can be used neat or with sand or aggregates. Uses: Resurfacing concrete and masonry; Mixing with sand and gravel for grouts; Filling pot holes and cracks; Leveling severely spalled surfaces; Resurfacing driveways; Weatherproof cable embedments in floors; Structural adhesive grouts. Advantages of AboTar 8607-1: Filling Pot Holes and Gaps with a structurally tough, yet less expensive epoxy/aggregate mix; Making Concrete-Substitute Mixes where more strength than concrete is needed, and where structural pourings must be made that bond permanently where concrete cannot bond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity <= 8000 cP<= 8000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 82.222 - 98.889 °C
1.00 - 2.00 hour
@Temperature 180.00 - 210.00 °F
 5760 - 8640 min
@Temperature 15.556 - 26.667 °C
96.0 - 144 hour
@Temperature 60.001 - 80.001 °F
(4-6 Days)
Pot Life <= 45 min<= 45 min
 
Descriptive Properties
Hardening Time (min)120-600at ambient temp.; faster with heating
Induction Period (min)>= 15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder
Gypsum (CaSO4 - 2H2O)

PABC910 / 107894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.