MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin.
- Black: A-1145 HS BK 324
- Natural: A-1145 HS NT

Key Attributes: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Strength; High Temperature Strength; Low Moisture Absorption

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve Parts

Automotive Specifications: 3M 11-0003-5762-1 Color: BK324 Black; ASTM D4000 PA121 G45 Color: BK324 Black; ASTM D4000 PA121 G45 Color: NT Natural; ASTM D4000 PPA0120 G46 A95726 AA002 CD295 GB159 MF015Z Color: BN575 Brown; ASTM D6779 PA121G45; BOSCH 9 916 365 011 Color: BK 324 Black; BOSCH 9 916 365 011 Color: NT Natural; CHRYSLER MS-DB-478 Type B CPN3567 Color: Black; FORD WSB-M4D861-A Color: BK324 Black; FORD WSB-M4D861-A Color: NT Natural; GM GMP.PPA.008 Color: BK324 Black; GM GMP.PPA.008 Color: NT Natural; GM GMW16356P-PPA-GF45 Color: BK-324 Black; GM GMW16356P-PPA-GF45 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 12-160, GF45 Color: NT Natural; TRW S-13301201 Color: BK324 Black

Injection Notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. Manufacturer recommendeds that Amodel® resins be dried prior to molding.

Data for dry samples unless noted.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ISO 1183, Method A
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D255
  • Linear Mold Shrinkage, Transverse, ASTM D255
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength, ASTM D638, Conditioned
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638, Conditioned
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ASTM D638, Conditioned
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ASTM D790, Conditioned
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790, Conditioned
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Poissons Ratio, ASTM E132
  • Shear Strength, ASTM D732, Conditioned
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256, Conditioned
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180, Type 1, Notch A
  • Izod Impact, Unnotched (ISO), ISO 180, Type 1, Notch A
  • Charpy Impact Unnotched, ISO 179, Type 1, Edgewise
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Volume Resistivity, ASTM D257, Conditioned
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150, Conditioned
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150, Conditioned
  • Dielectric Strength, ASTM D149, Conditioned
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150, Conditioned
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150, Conditioned
  • Arc Resistance, ASTM D495, Conditioned
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, UL 746, Conditioned
  • Comparative Tracking Index, UL 746
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Melting Point, ASTM D3418, Peak
  • Melting Point, ISO 11357-3
  • Maximum Service Temperature, Air, ASTM D794, Continuous
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Flammability, UL94, UL 94
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.