Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. - Black: A-1145 HS BK 324 - Natural: A-1145 HS NTKey Attributes: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Strength; High Temperature Strength; Low Moisture Absorption Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve Parts Automotive Specifications: 3M 11-0003-5762-1 Color: BK324 Black; ASTM D4000 PA121 G45 Color: BK324 Black; ASTM D4000 PA121 G45 Color: NT Natural; ASTM D4000 PPA0120 G46 A95726 AA002 CD295 GB159 MF015Z Color: BN575 Brown; ASTM D6779 PA121G45; BOSCH 9 916 365 011 Color: BK 324 Black; BOSCH 9 916 365 011 Color: NT Natural; CHRYSLER MS-DB-478 Type B CPN3567 Color: Black; FORD WSB-M4D861-A Color: BK324 Black; FORD WSB-M4D861-A Color: NT Natural; GM GMP.PPA.008 Color: BK324 Black; GM GMP.PPA.008 Color: NT Natural; GM GMW16356P-PPA-GF45 Color: BK-324 Black; GM GMW16356P-PPA-GF45 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 12-160, GF45 Color: NT Natural; TRW S-13301201 Color: BK324 Black Injection Notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. Manufacturer recommendeds that Amodel® resins be dried prior to molding. Data for dry samples unless noted. Information provided by Solvay Specialty Polymers. |