MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Danquinsa DANTHANE® 125H-Powder Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANTHANE_ 125H-Powder is a polyester based, thermoplastic, aromatic structured TPU-powder. DANTHANE_ 125H-Powder distinguish itself by its low softening point and its good adhesive behaviour. DANTHANE_ 125H-Powder is applied by melt calender coating of textiles or other supporting materials. This TPU can be processed by sinter coating as well as by flatbed and transfer calender lamination. Typical applications for this product are:
  • Adhesive equipment for seam sealing tapes
  • Lamination of textiles with different décor Films
  • Thermobond equipment of textiles
Application: DANTHANE_ 125H-Powder is mainly used as adhesive powder for adhesive equipment as well as for coating and lamination of textiles and other supporting materials. Adhesive coatings, produced with DANTHANE_ 125H-Powder distinguish itself by an excellent reaction and sealing behaviour. Also the thermal welding of adhesive equipments is given. DANTHANE_ 125H-Powder is used for thermobond equipments of different textiles needed for example as label, adhesive label etc. The product is best suitable for coatings and laminations of different products. This powder is also very suitable for the thermobond equipment of textiles, plastic adhesive tapes and materials for seam sealing.

Information provided by Danquinsa GMBH

Vendors:
Available Properties
  • Density, DIN 53.479
  • Particle Size, Powder grit size
  • Viscosity, DIN 53.735
  • Brookfield Viscosity, 20% in THF, RVT, spindle 3, 20 U.p.M./20°C
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • Hardness, Shore A, DIN 53.505
  • Tensile Strength, DIN 53.504
  • Elongation at Break, DIN 53.504
  • 100% Modulus, DIN 53.504
  • 200% Modulus, DIN 53.504
  • 300% Modulus, DIN 53.504
  • Abrasion, DIN 53.516, [mm³]
  • Compression Set, DIN 53.517
  • Compression Set, DIN 53.517
  • Melting Point, Kofler
  • Softening Point, Kofler
  • Glass Transition Temp, Tg, DIN 51.513, DSC
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.