MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Arla MULTICLEAR® STRONG 6Wall PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MULTICLEAR® STRONG 6Wall is a unique range of extruded multiwall polycarbonate sheets specifically designed to be low U-value product with increased stiffness, allowing cost saving and providing increased light transmittance due to less glazing bars required for installation. MULTICLEAR® STRONG 6Wall is a transparent or translucent sheet with one or two sides UV protection. Standard production available in thickness 8, 10 and 16 mm, in clear, opal and bronze color. Dust free knife cutting is used in all formatting operations. MULTICLEAR® STRONG 6Wall has a 10 years limited warranty against discoloration, loss of impact strength and light transmission due to weathering. Excellent fire performance: In case of fire, the sheet will melt and allow venting where heat and smoke will be let out and therefore reduce the growth of fire by flame spread. Classification B-s1,d0 according to EN 13501-1 ( Fire classification of construction products and building elements -reaction to fire tests)

Benefits: High light transmission; Outstanding bending radius; Cross structure offering increased stiffness; Excellent thermal insulation

Application: Building industry – roofing, cladding, sidewalls, conservatories, domes, skylights, sheds, carports, smoke vents, swimming pool covers, suspended ceilings, glasshouses, shopping center roofing, railway/metro station, stadia roofing and partitions; Agriculture greenhouses, lorry /tractor ports and farm/barn buildings; Packaging boxes for lamp optics, neon signs, pallet shields and protective covers for fragile items; Advertising illuminated signs and panels.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 50% RH
  • Hardness, Rockwell M, ISO 2039-2
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact Unnotched, ISO 179/2D
  • Charpy Impact Unnotched, ISO 179/2D
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, DIN 52612
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306, B 50
  • Vicat Softening Point, ISO 306, B 120
  • Refractive Index, ISO 489
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.