MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned  (Unverified Data**)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping behavior.

Key Words: Polyamide; Poly(Acrylonitrile-Butadiene-Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccdry as molded
Linear Mold Shrinkage 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength, Yield 30.0 MPa
Elongation at Break 190 %ASTM D638
Elongation at Yield 13 %
Tensile Modulus 1.03 GPa
Flexural Yield Strength 57.0 MPaat 5% strain; ASTM D790
Flexural Modulus 1.20 GPaASTM D790
Izod Impact, Notched 8.00 J/cm
@Thickness 3.20 mm
ASTM D256
 0.800 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM D256
Charpy Impact Unnotched NB
 1.60 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 7.40 J/cm²
Impact Test 42.0 J
@Thickness 2.50 mm
Instrumented Total Impact; 2.5 mm thick, 12.5 mm dart, 40 mm clamp, 3.3 m/s; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 9.00e+12 ohm-cmASTM D257
Surface Resistance 3.20e+13 ohmASTM D257
Dielectric Constant 3.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 1.60 mm
Short time under oil; ASTM D149
Dissipation Factor 0.039
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 sec
@Thickness 3.18 mm
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index >= 600 V
@Thickness 3.18 mm
UL Rating PLC 0 (>600 V)
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 3.18 mm
UL Rating PLC 2 (30-60 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.57 mm
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min
@Thickness 3.18 mm
UL Rating PLC 0 (<10 mm/min.)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
Vicat Softening Point 98.0 °C
UL RTI, Electrical 110 °C
UL RTI, Mechanical with Impact 65.0 °C
UL RTI, Mechanical without Impact 105 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 46, Unreinforced
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 63, 35% Glass-Filled
INEOS Styrolution Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

PBA591 / 27029

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.