MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon 6, 10% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.80 g/cc0.0397 - 0.0650 lb/in³Average value: 1.23 g/cc Grade Count:213
 1.067 - 1.067 g/cc
@Temperature >=220 °C
0.03855 - 0.03855 lb/in³
@Temperature >=428 °F
Average value: 1.07 g/cc Grade Count:2
Filler Content 5.00 - 30.0 %5.00 - 30.0 %Average value: 11.6 % Grade Count:30
Water Absorption 0.0900 - 8.30 %0.0900 - 8.30 %Average value: 2.18 % Grade Count:87
Moisture Absorption at Equilibrium 1.20 - 3.00 %1.20 - 3.00 %Average value: 2.31 % Grade Count:33
 2.00 - 3.40 %
@Temperature 70.0 - 70.0 °C
2.00 - 3.40 %
@Temperature 158 - 158 °F
Average value: 2.80 % Grade Count:5
Water Absorption at Saturation 6.30 - 9.50 %6.30 - 9.50 %Average value: 7.88 % Grade Count:21
Viscosity 2.60 - 50.0 cP2.60 - 50.0 cPAverage value: 12.3 cP Grade Count:5
Viscosity Test 145 - 150 cm³/g1.45 - 1.50 dl/gAverage value: 146 cm³/g Grade Count:6
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.136 Grade Count:8
 0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.0200 cm/cm0.00200 - 0.0200 in/inAverage value: 0.00666 cm/cm Grade Count:144
 0.00500 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
0.00500 - 0.00500 in/in
@Temperature 176 - 176 °F
Average value: 0.00500 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00100 - 0.0197 cm/cm0.00100 - 0.0197 in/inAverage value: 0.0103 cm/cm Grade Count:44
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00800 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00800 cm/cm Grade Count:2
Melt Flow 2.00 - 93.8 g/10 min2.00 - 93.8 g/10 minAverage value: 27.0 g/10 min Grade Count:21
Ash 0.500 - 13.0 %0.500 - 13.0 %Average value: 7.72 % Grade Count:5
 18.0 - 22.0 %
@Temperature 625 - 625 °C
18.0 - 22.0 %
@Temperature 1160 - 1160 °F
Average value: 20.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 94.0 - 12194.0 - 121Average value: 111 Grade Count:5
Hardness, Rockwell R 100 - 122100 - 122Average value: 119 Grade Count:42
Ball Indentation Hardness 95.0 - 155 MPa13800 - 22500 psiAverage value: 127 MPa Grade Count:3
Tensile Strength, Ultimate 3.45 - 200 MPa500 - 29000 psiAverage value: 90.6 MPa Grade Count:166
 20.0 - 170 MPa
@Temperature -40.0 - 150 °C
2900 - 24700 psi
@Temperature -40.0 - 302 °F
Average value: 76.8 MPa Grade Count:9
Tensile Strength, Yield 51.7 - 162 MPa7500 - 23500 psiAverage value: 99.2 MPa Grade Count:54
Elongation at Break 1.60 - 30.0 %1.60 - 30.0 %Average value: 5.19 % Grade Count:189
 2.00 - 30.0 %
@Temperature -40.0 - 150 °C
2.00 - 30.0 %
@Temperature -40.0 - 302 °F
Average value: 9.81 % Grade Count:9
Elongation at Yield 2.00 - 15.0 %2.00 - 15.0 %Average value: 5.44 % Grade Count:21
Modulus of Elasticity 1.90 - 11.5 GPa276 - 1670 ksiAverage value: 4.70 GPa Grade Count:77
 1.445 - 6.90 GPa
@Temperature -40.0 - 150 °C
209.6 - 1000 ksi
@Temperature -40.0 - 302 °F
Average value: 3.46 GPa Grade Count:8
Flexural Yield Strength 13.8 - 300 MPa2000 - 43500 psiAverage value: 136 MPa Grade Count:181
 49.987 - 265 MPa
@Temperature -40.0 - 121 °C
7250.0 - 38400 psi
@Temperature -40.0 - 250 °F
Average value: 147 MPa Grade Count:5
Flexural Modulus 1.52 - 10.6 GPa220 - 1540 ksiAverage value: 4.14 GPa Grade Count:194
 0.992845 - 5.19865 GPa
@Temperature -40.0 - 121 °C
144.002 - 754.012 ksi
@Temperature -40.0 - 250 °F
Average value: 2.30 GPa Grade Count:3
Izod Impact, Notched 0.300 - 1.95 J/cm0.562 - 3.65 ft-lb/inAverage value: 0.709 J/cm Grade Count:91
 0.37373 - 0.400 J/cm
@Temperature -40.0 - -40.0 °C
0.70015 - 0.749 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.391 J/cm Grade Count:3
Izod Impact, Unnotched 0.481 - 5.34 J/cm0.900 - 10.0 ft-lb/inAverage value: 4.22 J/cm Grade Count:12
Izod Impact, Notched (ISO) 3.00 - 19.9 kJ/m²1.43 - 9.49 ft-lb/in²Average value: 7.81 kJ/m² Grade Count:64
 5.00 - 8.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.38 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 38.0 - 38.0 kJ/m²
@Temperature -30.0 - -30.0 °C
18.1 - 18.1 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 38.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 J/cm² - NB9.52 ft-lb/in² - NBAverage value: 5.26 J/cm² Grade Count:51
 1.50 J/cm² - NB
@Temperature -40.0 - -20.0 °C
7.14 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 3.92 J/cm² Grade Count:28
Charpy Impact, Notched 0.100 - 2.20 J/cm²0.476 - 10.5 ft-lb/in²Average value: 0.776 J/cm² Grade Count:112
 0.100 - 1.39 J/cm²
@Temperature -40.0 - -20.0 °C
0.476 - 6.62 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.485 J/cm² Grade Count:30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 - 1.00e+18 ohm-cm1.00 - 1.00e+18 ohm-cmAverage value: 1.84e+16 ohm-cm Grade Count:61
Surface Resistance 10.0 - 1.00e+15 ohm10.0 - 1.00e+15 ohmAverage value: 9.06e+13 ohm Grade Count:27
Static Decay 2.00 sec2.00 secAverage value: 2.00 sec Grade Count:4
Shielding Effectiveness 50.0 dB50.0 dBAverage value: 50.0 dB Grade Count:3
Dielectric Constant 3.00 - 7.003.00 - 7.00Average value: 4.20 Grade Count:16
Dielectric Strength 7.87 - 80.0 kV/mm200 - 2030 kV/inAverage value: 23.2 kV/mm Grade Count:30
Dissipation Factor 0.0100 - 0.07000.0100 - 0.0700Average value: 0.0250 Grade Count:9
Arc Resistance 112 - 160 sec112 - 160 secAverage value: 136 sec Grade Count:4
Comparative Tracking Index 225 - 600 V225 - 600 VAverage value: 483 V Grade Count:28
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 97.0 µm/m-°C7.78 - 53.9 µin/in-°FAverage value: 44.9 µm/m-°C Grade Count:41
CTE, linear, Transverse to Flow 12.0 - 95.0 µm/m-°C6.67 - 52.8 µin/in-°FAverage value: 70.0 µm/m-°C Grade Count:10
Specific Heat Capacity 1.40 - 2.73 J/g-°C0.335 - 0.652 BTU/lb-°FAverage value: 2.06 J/g-°C Grade Count:4
Thermal Conductivity 0.230 - 20.0 W/m-K1.60 - 139 BTU-in/hr-ft²-°FAverage value: 3.52 W/m-K Grade Count:7
Melting Point 210 - 315 °C410 - 599 °FAverage value: 221 °C Grade Count:92
Maximum Service Temperature, Air 85.0 - 200 °C185 - 392 °FAverage value: 135 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 180 - 260 °C356 - 500 °FAverage value: 210 °C Grade Count:80
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 302 °C149 - 576 °FAverage value: 187 °C Grade Count:160
Vicat Softening Point 170 - 250 °C338 - 482 °FAverage value: 204 °C Grade Count:25
Flammability, UL94 HB - V-0HB - V-0Grade Count:104
Oxygen Index 22.0 - 24.0 %22.0 - 24.0 %Average value: 23.0 % Grade Count:4
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 768 °C Grade Count:13
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 275 °C176 - 527 °FAverage value: 235 °C Grade Count:21
Nozzle Temperature 230 - 293 °C446 - 560 °FAverage value: 261 °C Grade Count:20
Melt Temperature 210 - 304 °C410 - 580 °FAverage value: 260 °C Grade Count:91
Mold Temperature 21.1 - 121 °C70.0 - 250 °FAverage value: 80.1 °C Grade Count:98
Injection Velocity 30.0 - 60.0 mm/sec1.18 - 2.36 in/secAverage value: 50.0 mm/sec Grade Count:4
Drying Temperature 65.6 - 130 °C150 - 266 °FAverage value: 82.1 °C Grade Count:76
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.155 % Grade Count:32
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -23.3 °C Grade Count:4
Injection Pressure 3.45 - 172 MPa500 - 25000 psiAverage value: 58.2 MPa Grade Count:38
Vent Depth 0.00127 - 0.00762 cm0.000500 - 0.00300 inAverage value: 0.00275 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for Nylon 6, 40% Glass Fiber Filled

O2411 / 77971

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.