MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® HTplus M1034 black E70285 Polyphthalamide (PPA), 40% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Glass fiber-reinforced, laser-weldable polyphthalamide compound. VESTAMID® HTplus M1034 black E70285 (similar like RAL 8022) is a glass fiber-reinforced, heat-stabilized polyphthalamide compound (PPA) with good IR-laser transparency for injection molding. The material contains about 40% glass fibers, an aging protective agent and processing aid for a fast and even form filling. VESTAMID® HTplus M1034 black E70285 is laser-weldable by a diode-pumped or solid-state laser in the range of ? = 808-1064 nm. The transparency level of VESTAMID® HTplus M1034 black E70285 can be influenced with the mold temperature during the injection molding process. With lower mold temperatures of 140°C the laser transparency can be increased up to 25% compared to higher temperatures of 180°C. Depending on the used mold temperature the processing shrinkage may vary slightly and therefore has to be considered regarding mold dimensions. The mechanical properties are not influenced. VESTAMID® HTplus M1034 black E70285 is supplied as cylindrical pellets in polyethylene packaging. Drying at 120°C for at least 4 hours before processing is recommended.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psiISO 527
Elongation at Break 1.7 %1.7 %ISO 527
Tensile Modulus 13.0 GPa1890 ksiISO 527
Charpy Impact Unnotched  3.30 J/cm²
@Temperature -30.0 °C
15.7 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 309 °C588 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 305 °C581 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/-2
Vicat Softening Point 279 °C534 °FMethod B: 10 N, 50 K/h; ISO 306
 309 °C588 °FMethod A: 10 N, 50 K/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 330 °C626 °FTest condition for mold shrinkage
Mold Temperature 160 °C320 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK835 / 243044

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.