MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU) (Extended Aging Data)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Texin 245 resin is an aromatic polyester-based thermoplastic polyurethane with a Shore hardness of approximately 43D. It can be processed by injection molding; extrusion processes are not recommended.

Properties / Applications: Texin 245 resin is characterized by excellent low-temperature properties and excellent fuel and oil resistance. It also offers outstanding abrasion resistance, impact strength, toughness, and flexibility. Texin 245 natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. Typical applications include casters, couplings, sleeves and gears.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43ASTM D2240
 32
@Time 252000 sec
Fuel C; ASTM D471
 32
@Time 605000 sec
Fuel C; ASTM D471
 32
@Time 1.21e+6 sec
Fuel C; ASTM D471
 32
@Time 1.81e+6 sec
Fuel C; ASTM D471
 41
@Time 252000 sec
Fuel A; ASTM D471
 41
@Time 605000 sec
Fuel A; ASTM D471
 42
@Time 1.81e+6 sec
Fuel A; ASTM D471
 43
@Time 1.21e+6 sec
Fuel A; ASTM D471
 38
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
 38
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
 38
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 39
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 39
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 40
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; ASTM D573
 40
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 40
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 40
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 40
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #3; ASTM D471
 40
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
 41
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #3; ASTM D471
Tensile Strength at Break 54.5 MPaASTM D412
 43.055 MPa
@Time 252000 sec
Fuel C; ASTM D471
 44.145 MPa
@Time 1.21e+6 sec
Fuel C; ASTM D471
 44.69 MPa
@Time 1.81e+6 sec
Fuel C; ASTM D471
 44.69 MPa
@Time 605000 sec
Fuel C; ASTM D471
 54.5 MPa
@Time 1.21e+6 sec
Fuel A; ASTM D471
 57.77 MPa
@Time 605000 sec
Fuel A; ASTM D471
 58.315 MPa
@Time 1.81e+6 sec
Fuel A; ASTM D471
 60.045 MPa
@Time 252000 sec
Fuel A; ASTM D471
 46.87 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
 49.05 MPa
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
 55.045 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 55.045 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
 57.225 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; ASTM D573
 57.225 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 58.86 MPa
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 59.405 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 62.13 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 62.675 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 64.31 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #3; ASTM D471
 65.4 MPa
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #3; ASTM D471
Tensile Stress at Strain 7.60 MPa
@Strain 50 %
ASTM D412
 9.00 MPa
@Strain 100 %
ASTM D412
 20.7 MPa
@Strain 300 %
ASTM D412
 8.73 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #1, 336; ASTM D471
 8.82 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #1, 70; ASTM D471
 8.91 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #1, 168; ASTM D471
 9.00 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #1, 50; ASTM D471
 9.18 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 504; ASTM D573
 9.18 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #3, 70; ASTM D471
 9.18 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #3, 504; ASTM D471
 9.27 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 168; ASTM D573
 9.27 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 336; ASTM D573
 9.27 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #3, 168; ASTM D471
 9.36 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 70; ASTM D573
 9.36 MPa
@Strain 100 %,
Temperature 100 °C
ASTM Oil #3, 336; ASTM D471
 18.837 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 50; ASTM D471
 19.665 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 336; ASTM D471
 19.872 MPa
@Strain 300 %,
Temperature 100 °C
Hot Air, 336; ASTM D573
 20.286 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 168; ASTM D471
 20.286 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 504; ASTM D471
 20.493 MPa
@Strain 300 %,
Temperature 100 °C
Hot Air, 504; ASTM D573
 20.7 MPa
@Strain 300 %,
Temperature 100 °C
Hot Air, 70; ASTM D573
 21.114 MPa
@Strain 300 %,
Temperature 100 °C
Hot Air, 168; ASTM D573
 21.114 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 70; ASTM D471
 21.114 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 336; ASTM D471
 22.77 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 168; ASTM D471
 22.977 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 70; ASTM D471
 7.11 MPa
@Time 252000 sec,
Strain 100 %
Fuel C; ASTM D471
 7.56 MPa
@Strain 100 %,
Time 605000 sec
Fuel C; ASTM D471
 7.65 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel C; ASTM D471
 7.74 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel C; ASTM D471
 8.82 MPa
@Strain 100 %,
Time 605000 sec
Fuel A; ASTM D471
 8.91 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel A; ASTM D471
 9.00 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel A; ASTM D471
 9.09 MPa
@Time 252000 sec,
Strain 100 %
Fuel A; ASTM D471
 13.662 MPa
@Time 252000 sec,
Strain 300 %
Fuel C; ASTM D471
 14.904 MPa
@Time 605000 sec,
Strain 300 %
Fuel C; ASTM D471
 14.904 MPa
@Strain 300 %,
Time 1.81e+6 sec
Fuel C; ASTM D471
 15.111 MPa
@Strain 300 %,
Time 1.21e+6 sec
Fuel C; ASTM D471
 19.665 MPa
@Time 605000 sec,
Strain 300 %
Fuel A; ASTM D471
 20.079 MPa
@Strain 300 %,
Time 1.81e+6 sec
Fuel A; ASTM D471
 20.7 MPa
@Strain 300 %,
Time 1.21e+6 sec
Fuel A; ASTM D471
 21.321 MPa
@Time 252000 sec,
Strain 300 %
Fuel A; ASTM D471
Elongation at Break 500 %ASTM D412
 460 %
@Time 605000 sec
Fuel C; ASTM D471
 470 %
@Time 605000 sec
Fuel A; ASTM D471
 475 %
@Time 1.81e+6 sec
Fuel C; ASTM D471
 480 %
@Time 252000 sec
Fuel A; ASTM D471
 480 %
@Time 1.21e+6 sec
Fuel C; ASTM D471
 485 %
@Time 1.21e+6 sec
Fuel A; ASTM D471
 490 %
@Time 1.81e+6 sec
Fuel A; ASTM D471
 495 %
@Time 252000 sec
Fuel C; ASTM D471
 500 %
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; ASTM D573
 510 %
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 510 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 515 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 525 %
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #3; ASTM D471
 525 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 530 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
 540 %
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 550 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
 550 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #3; ASTM D471
 550 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 595 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
Flexural Modulus 51.7 MPa
@Temperature 70.0 °C
ASTM D790
 68.9 MPa
@Temperature 23.0 °C
ASTM D790
Compressive Strength 0.700 MPa2% Deflection; ASTM D 575
 2.10 MPa5% Deflection; ASTM D 575
 3.90 MPa10% Deflection; ASTM D 575
 5.50 MPa15% Deflection; ASTM D 575
 6.90 MPa20% Deflection; ASTM D 575
 9.00 MPa25% Deflection; ASTM D 575
 23.0 MPa50% Deflection; ASTM D 575
Resilience 45[%], Bayshore; ASTM D2632
Izod Impact, Notched 3.30 ft-lb/in
@Thickness -762 mm
ASTM D256
 NB
@Thickness 584 mm
ASTM D256
Tear Strength 122.6 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 70
@Load 1.00 kg
[mg] Loss, H-18; ASTM D3489
Compression Set 18 %
@Temperature 23.0 °C,
Time 79200 sec
as molded; ASTM D395-B
 18 %
@Temperature 23.0 °C,
Time 79200 sec
postcured; ASTM D395-B
 35 %
@Temperature 100 °C,
Time 79200 sec
postcured; ASTM D395-B
 35 %
@Temperature 70.0 °C,
Time 79200 sec
postcured; ASTM D395-B
 43 %
@Temperature 70.0 °C,
Time 79200 sec
as molded; ASTM D395-B
 60 %
@Temperature 100 °C,
Time 79200 sec
as molded; ASTM D395-B
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 148 °CRate A; ASTM D1525
Brittleness Temperature >= -90.0 °FASTM D746
Glass Transition Temp, Tg -46.0 °C
UL RTI, Electrical 50.0 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 193 - 204 °C
Middle Barrel Temperature 193 - 204 °C
Front Barrel Temperature 199 - 210 °C
Nozzle Temperature 204 - 210 °C
Melt Temperature 204 - 216 °C
Mold Temperature 15.0 - 40.0 °C
Injection Pressure 6000 - 15000 psi
Back Pressure <= 200 psi
Cushion <= 0.125 in
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane
Covestro Desmopan® DP 8785 A Polyurethane
Covestro Desmopan® 6064A TPU
Covestro Desmopan® 3055D Polyurethane

PCOVEST0974a / 238178

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.