MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lord Adhesives 7421 Urethane Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7421 adhesive is a single-component, moisture-cure urethane adhesive offering quality adhesion performance and non-conductive properties. It successfully bonds Hytrel®, chlorinated polyethylene (CPE), thermoplastic polyurethane (TPU), Nylon 11 and other thermoplastics to fiber reinforcements, such as polyester and Kevlar®, during construction of high-pressure hose. LORD 7421 adhesive adheres reinforcement yarns to the extruded core, as well as adhering the extruded jacket to the reinforcement yarns. This single-component adhesive provides good hydrolytic stability and has an increased working life. Hytrel and Kevlar are trademarks of DuPont. After opening, protect adhesive from excessive exposure to moisture by using dry nitrogen as an inert cover each time material is removed. Do not return dispensed material to its original container. The viscosity of this product will increase over time.

Features: easy to see on light colored substrates. provides high elongation, modulus and tensile strength. requires no mixing; provides long working time with minimum waste; requires no ovens or other heat source for curing. resists sunlight, weathering, humidity and salt spray. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0422 lb/in³
Solids Content 70 %70 %by weight
 71.8 %71.8 %by volume
Brookfield Viscosity 550 - 1550 cP
@Temperature 25.0 °C
550 - 1550 cP
@Temperature 77.0 °F
Brookfield HAT, Spindle 2, 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.6 MPa4000 psicured
Elongation at Break 360 %360 %cured; ASTM D882-A3A, modified)
Modulus of Elasticity 0.124 GPa18.0 ksi
Tear Strength 100.7 kN/m574.6 pli
Peel Strength 3.51 - 5.26 kN/m20.0 - 30.0 pliversus polyester fabric; ASTM 1876-72
 9.64 - 11.4 kN/m55.0 - 65.0 pliversus Hytrel 5556; ASTM 1876-72
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FSeta
 
Descriptive Properties
AppearanceGreen/grey liquid
SolventsMethylene Chloride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9125 / 232513

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.