MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ASI® MP 5400 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP5400 is a one component, heat curable thixotropic paste epoxy adhesive. It is a non-sag adhesive which forms strong bonds to metals and ceramics. MP5400 has exceptional thermal stability and resistance to water, humidity and solvents. This product offers high heat resistance and cures rapidly in either a convection oven or infra-red oven. MP5400 readily exceeds all requirements of military specifications MMMA-132 for type II heat resistant structural adhesives.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc
@Temperature 25.0 °C
1.41 g/cc
@Temperature 77.0 °F
Viscosity 700000 - 900000 cP
@Temperature 25.0 °C
700000 - 900000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  75
@Temperature 120 °C
75
@Temperature 248 °F
 85
@Temperature 25.0 °C
85
@Temperature 77.0 °F
Tensile Strength >= 44.1 MPa>= 6400 psi
Elongation at Break >= 1.5 %>= 1.5 %
Adhesive Bond Strength >= 21.4 MPa>= 3100 psiLap Shear
Izod Impact, Notched 0.192 J/cm0.360 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 56.0 µm/m-°C31.1 µin/in-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 148 °C298 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 121 °C
0.0333 hour
@Temperature 250 °F
 10.0 min
@Temperature 149 °C
0.167 hour
@Temperature 300 °F
 15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F
Shelf Life  0.500 Month
@Temperature 38.0 °C
0.500 Month
@Temperature 100 °F
 6.00 Month
@Temperature 24.0 °C
6.00 Month
@Temperature 75.2 °F
 12.0 Month
@Temperature <=0.000 °C
12.0 Month
@Temperature <=32.0 °F
Store in a cool, dry area
 
Descriptive Properties
Color / appearancegray
Press Flow60-80 sec
Sag Resistance0.375"-0.42"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9099 / 233466

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.