MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChenGuang Hexafluoropropylene (HFP)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Chemical formula: CF2=CF-CF3

CAS No.: 116-15-4

Description: HFP is one of the important monomers of fluoropolymers. It could react with VdF to make fluoroelastomer copolymer, with TFE and VdF to make fluoroelastomer terpolymer, and with TFE to make FEP. All these fluorinated polymers are special chemicals necessary for modern industries. HFP is the essential raw material of the new and pollutionless extinguishing agent F227.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.332 g/cc1.332 g/ccLiquid
Molecular Weight 150.021 g/mol150.021 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point -29.4 °C
@Pressure 1.013e+8 MPa
-20.9 °F
@Pressure 1.469e+10 psi
 
Component Elements PropertiesMetricEnglishComments
Oxygen, O <= 50 %<= 50 %
 
Descriptive Properties
Acidity (HF)<0.1 ppmQFBX - J
 <0.1 ppmQFBX - M
Content<0.1 ppmPerfluoroisobutene, QFBX - J
 <2000 ppmUn-saturated fluorocarbon compounds, QFBX - M
 <3000 ppmSaturated fluorocarbon compounds, QFBX - M
 <5000 ppmUn-saturated fluorocarbon compounds, QFBX - J
 <5000 ppmSaturated fluorocarbon compounds, QFBX - J
 >99.5%HFP, QFBX - J, QFBX - M
Freezing Point-156.2°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU040 / 255639

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.