MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-EXP-002 Fluoroelastomer Copolymer, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-EXP-002 is a cure incorporated copolymer with medium-low Mooney viscosity. It is designed for injection molding of o-rings, seals and other parts where fast curing and low compression set are required. DAI-EL® G-EXP-002 may be used in compliance with 21 CFR 177.2600, Rubber articles intended for repeated use. Finished articles are required to comply with the end tests specified in 21 CFR 177.2600 (e) or (f), as applicable.

Typical Applications: O-rings, seals, gaskets, molded tubing

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/cc
Mooney Viscosity 33
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 16.5 MPa
Elongation at Break 200 %
100% Modulus 7.20 MPa
@Strain 100 %
Compression Set 15.4 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -18.0 °CLow Temperature Retraction; ASTM D1329
 
Processing PropertiesOriginal ValueComments
Cure Time 1.30 mints2, scorch time
 1.50 mint'50, time to 50% cure
 2.50 mint'90, time to 90% cure
 10.0 min
@Temperature 177 °C
Press Cure
 24.0 hour
@Temperature 232 °C
Post Cure
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
ColorWhite to cream
MH26.4 dNmmaximum torque
ML1.1 dNmminimum torque
Test Formula100 phrDAI-EL® G-EXP-002
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Fluoroelastomer
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Grolltex Large Area CVD Graphene Film on Copper, 6" x 6" (150mm x 150mm)
Daikin NEOFLON® NP-112 FEP
CHT Group QSil 229LV Transparent, Liquid Silicone Rubber

PDAIJ9800 / 209871

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.