MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 229LV Transparent, Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product Description: QSil 229LV is a two-part, heat cured, optically clear liquid silicone which exhibits great transmittance. It has a low viscosity which allows for ease of flow around complex parts, providing electrical insulation and shock resistance. The product exhibits good adhesion to most surfaces.

Key Features:

  • Convenient 1:1 mixing ratio for use in automatic dispensing equipment or hand mixing
  • Contains no solvents
  • Non-yellowing catalyst system
  • Heat cure required to obtain full properties and adhesion

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncatalyzed, QSil 229LV A
 1.00 g/cc1.00 g/ccUncatalyzed, QSil 229LV B
Viscosity 1100 cP1100 cPUncatalyzed, QSil 229LV A
 9500 cP9500 cPUncatalyzed, QSil 229LV B
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inCured 60 minutes @ 150°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565Cured 60 minutes @ 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cm
Dielectric Constant 2.69
@Frequency 1000 Hz
2.69
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.00060
@Frequency 1000 Hz
0.00060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 275 µm/m-°C153 µin/in-°F
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4051.405
Transmission, Visible >= 98 %
@Thickness 1.00 mm,
Wavelength 400 nm
>= 98 %
@Thickness 0.0394 in,
Wavelength 400 nm
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 120 min
@Temperature 120 °C
2.00 hour
@Temperature 248 °F
 
Descriptive Properties
ColorClearCatalyzed
 Clear to cloudyUncatalyzed, QSil 229LV A
 Clear to cloudyUncatalyzed, QSil 229LV B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 229 Transparent, Liquid Silicone Rubber
Rogers Arlon 31970XA015 Silicone Rubber Laminate
Rogers Arlon 25188T010 Silicone Rubber/Laminated ETFE Film
Overview of materials for Silicone Rubber
CHT Group QSil 223 Transparent, Liquid Silicone Rubber

PACC2088 / 199476

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.