MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa DANTHANE® 125H Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANTHANE_ 125H is a polyester based, thermoplastic, aromatic structured TPU-granule. DANTHANE_ 125H has the distinction by its low softening point and its good adhesive behaviour. DANTHANE® 125H is applied by melt calander coating of textiles or other supporting materials. DANTHANE_ 125H is used at the production of coated textiles as they were needed for example at:
  • sealing of seams
  • membrane foils
  • mattress coatings
  • good thermic welded foils
  • ?thermobond equipment
> Application: DANTHANE_ 125H is needed by the hot melt coating of industrial textiles. Coated textiles or even produced mono foils distinguishes themselves by their excellent reactivation behaviour and thermic welding behaviour. DANTHANE_ 125H is further best suitable for thermobonding equipment of textiles. By this kind of application it is possible to extrude the granules of DANTHANE_ 125H into films. Grinded to powder there is the possibility to apply the powder of DANTHANE_ 125H by spread coating, powder or dot point coating. Concerning powder we refer to the type DANTHANE_ 125H–Powder.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³DIN 53.479
Viscosity 1010 cP
@Load 2.16 kg,
Temperature 180 °C
1010 cP
@Load 4.76 lb,
Temperature 356 °F
DIN 53.735
Brookfield Viscosity 300 - 400 cP300 - 400 cP20% in THF, RVT, spindle 3, 20 U.p.M./20°C
Melt Flow  12 g/10 min
@Load 2.16 kg,
Temperature 160 °C
12 g/10 min
@Load 4.76 lb,
Temperature 320 °F
ISO 1133
 35 - 55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
35 - 55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585DIN 53.505
Tensile Strength 35.0 MPa5080 psiDIN 53.504
Elongation at Break 630 %630 %DIN 53.504
100% Modulus 5.00 MPa725 psiDIN 53.504
200% Modulus 6.00 MPa870 psiDIN 53.504
300% Modulus 7.00 MPa1020 psiDIN 53.504
Abrasion 2828[mm³]; DIN 53.516
Compression Set  30 %
@Temperature 23.0 °C,
Time 252000 sec
30 %
@Temperature 73.4 °F,
Time 70.0 hour
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
80 %
@Temperature 158 °F,
Time 24.0 hour
DIN 53.517
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 155 °C293 - 311 °FKofler
Softening Point 130 - 135 °C266 - 275 °FKofler
Glass Transition Temp, Tg -32.0 °C-25.6 °FDSC; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectTransparent to light yellow pearl granules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ133 / 294553

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.