MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECANAT® GF20 natural PC, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes:
  • high toughness
  • good thermal stability
  • very high stiffness
  • good tensile strength
Target Industries:
  • aircraft and aerospace technology
  • automotive industry
  • fixture construction
  • electrical engineering
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
Moisture Absorption 0.290 %saturation; ASTM D570
 0.0700 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 87ASTM D 785
Tensile Strength, Yield 11000 psiASTM D 638
Elongation at Break 3.0 %ASTM D 638
Modulus of Elasticity 700 ksiASTM D 638
Flexural Strength 16700 psiASTM D 790
Flexural Modulus 600000 psiASTM D 790
Compressive Yield Strength 15000 psi
@Strain 10 %
ASTM D 695
Compressive Strength 2000 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 319000 psiASTM D 695
Izod Impact, Unnotched 2.06 ft-lb/in
Coefficient of Friction, Dynamic 0.22
@Pressure 0.276 MPa
50 fpm; ASTM D 3702
K (wear) Factor 120 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D 257
Dielectric Constant 3.13
@Frequency 1e+6 Hz
ASTM D 150
 3.17
@Frequency 60 Hz
50% RH; ASTM D 150
Dielectric Strength 19.3 kV/mmASTM D 149
Dissipation Factor 0.00090
@Frequency 60 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µin/in-°F
@Temperature -40.0 - 95.0 °C
ASTM E 831
Maximum Service Temperature, Air 266 °FLong Term
 275 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 298 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 295 °FASTM D 648
Vicat Softening Point 329 °FASTM D1525
Flammability, UL94 V-0
 
Descriptive Properties
Colorblue grey opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8173 / 319101

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.