MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® Michem ® Flex B3510I Transparent oxygen barrier coating
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Transparent oxygen barrier coating for flexible packaging. Michem® Flex B3510I is designed to be applied to polymer materials using gravure or flexographic coating processes. Suggested coat weight is 0.3 dry gsm. At the recommended coating weight, the dried coating is transparent, non-blocking and contributes to oxygen barrier properties of polymer materials. It should be undiluted and dried thoroughly after application. A black light can be used to see the coating during application to confirm uniformity of the coating onto the substrate. Usage: A transparent, high oxygen barrier, water-based coating designed primarily for polymer materials that can also be combined with metallization processes as a protective oxygen barrier coating. Michem® Flex Barrier 3510I has a UV indicator added for better visibility of coating during application when used with a black light.

Applications (properties imparted): Functional Coatings oxygen barrier.

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 - 1.01 g/cc0.990 - 1.01 g/cc
Solids Content 9.5 - 10.5 %9.5 - 10.5 %Non-Volatiles
pH 3.0 - 6.03.0 - 6.0
Brookfield Viscosity 0.00 - 100 cP0.00 - 100 cPSpindle #1. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceClear yellowish to brownish, cloudy
Freeze/Thaw StabilityNone: protect from freezing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9835 / 287430

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.