MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 Type 6 (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Data provided by Quadrant Engineering Plastic Products

  • Broadest size range availability
  • Good mechanical and electrical properties
  • Ideal balance of strength and toughness
  • Cast as finished parts and near net shapes (nylon 6)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Water Absorption 0.60 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 7.0 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Hardness, Rockwell R 115ASTM D785
Hardness, Shore D 85ASTM D2240
Tensile Strength 12000 psiASTM D638
Tensile Strength at 65°C (150°F) 6000 psiASTM D638
Elongation at Break 20 %ASTM D638
Tensile Modulus 400 ksiASTM D638
Flexural Strength 16000 psiASTM D790
Flexural Modulus 500 ksiASTM D790
Compressive Strength 15000 psi10% Def.; ASTM D695
Compressive Modulus 400000 psiASTM D695
Shear Strength 11000 psiASTM D732
Izod Impact, Notched 0.400 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.20Dry vs. Steel; QTM55007
K (wear) Factor 100 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 500 V/milShort Term; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 2.37 BTU-in/hr-ft²-°FASTM F433
Melting Point 420 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 200 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 200 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ColorBlue
Machinability11-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM21Cc / 216141

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.