Mitsubishi Chemical Advanced Materials Nylatron™ MC 901 PA6
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Cast
Material Notes:
Nylatron™ MC 901 Polyamide PA6 shapes with its distinctive blue color exhibits higher toughness, flexibility and fatigue resistance than standard nylons. It has proved to be an excellent material for gear wheels, racks and pinions.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
85.0
85.0
ASTM D785
Hardness, Shore D
80.0
80.0
ISO 868
Tensile Strength
84.0
MPa
12200
psi
ISO 527-1/-2 (7)
Elongation at Yield
5.00 %
5.00 %
ISO 527-1/-2 (7)
Flexural Strength
131
MPa
19000
psi
ISO 178 (12)
Compressive Yield Strength
32.0
MPa
@Strain 1.00 %
4640
psi
@Strain 1.00 %
ISO 604 (10)
61.0
MPa
@Strain 2.00 %
8850
psi
@Strain 2.00 %
ISO 604 (10)
90.0
MPa
@Strain 5.00 %
13100
psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched
0.300
J/cm²
1.43
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Dielectric Strength
25.0
kV/mm
635
kV/in
IEC 60243-1 (15)
Thermal Properties
Metric
English
Comments
CTE, linear
80.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4
µin/in-°F
@Temperature 73.4 - 140 °F
90.0
µm/m-°C
@Temperature 23.0 - 100 °C
50.0
µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity
0.290
W/m-K
2.01
BTU-in/hr-ft²-°F
Minimum Service Temperature, Air
-30.0
°C
-22.0
°F
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Unacceptable
Unacceptable
Acids, Weak
Limited
Limited
Alcohols
Limited
Limited
Alkalies, Strong (pH 11-14)
Unacceptable
Unacceptable
Alkalies, Weak
Limited
Limited
Chlorinated Solvents
Limited
Limited
Continuous Sunlight
Limited
Limited
Hot Water / Steam
Limited
Limited
Hydrocarbons - Aliphatic
Acceptable
Acceptable
Hydrocarbons - Aromatic
Acceptable
Acceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Acceptable
Acceptable
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM21Cc / 216141
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.