High-temperature, high-performance epoxy formulation for synthetic composite part and tooling manufacture. Tg as high as 300°F (149°C) with proper post cure. Provides excellent temperature stability and great part cosmetics. Slow cure speed hardener provides 4 to 5 hours working time at 72°F (22°C). A typical laminate will gel in 8 to 10 hours at room temperature. Medium viscosity for wet out of synthetic composite fabrics. Elevated temperature cure is required. Parts can be pulled after 24-48 hours at room temperature or sooner after a mild initial cure of 90-110°F (32-43°C). See chart for post cure information. Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.Information provided by Gougeon Brothers, Inc. |