MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Densit® Ducorit® S5 Grout
Categories: Ceramic

Material Notes: The ultra high performance grout, Ducorit® is used for structural grouted connections in wind turbine foundations and oil & gas installations - both offshore and onshore. The core of the Ducorit® products is the unique Densit® Binder. The different properties of Ducorit® S1, Ducorit® S2, Ducorit®S5, Ducorit® S5R and Ducorit® D4 are obtained by adding aggregates such as quartz sand or bauxite. Ducorit® products are characterized by extreme strength and stiffness, making them a strong structural component and not just a filling material.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 18.7 lb/gal
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1000 psi
Modulus of Elasticity 60.0 GPaDynamic
 8000 ksiStatic Modulus
Flexural Strength 2600 psi
Compressive Strength 18850 psi
Poissons Ratio 0.19
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.559 %es,m,91. SKVB 0
 0.567 %es,i,91. SKVB 0
 
Descriptive Properties
Consistence ClassClass B24 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWDE9072 / 239582

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.