MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Densit® Ducorit® S5 Grout
Categories: Ceramic

Material Notes: The ultra high performance grout, Ducorit® is used for structural grouted connections in wind turbine foundations and oil & gas installations - both offshore and onshore. The core of the Ducorit® products is the unique Densit® Binder. The different properties of Ducorit® S1, Ducorit® S2, Ducorit®S5, Ducorit® S5R and Ducorit® D4 are obtained by adding aggregates such as quartz sand or bauxite. Ducorit® products are characterized by extreme strength and stiffness, making them a strong structural component and not just a filling material.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.24 g/cc0.0810 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 6.89 MPa1000 psi
Modulus of Elasticity 55.2 GPa8000 ksiStatic Modulus
 60.0 GPa8700 ksiDynamic
Flexural Strength 17.9 MPa2600 psi
Compressive Strength 130.0 MPa18850 psi
Poissons Ratio 0.190.19
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.559 %0.559 %es,m,91. SKVB 0
 0.567 %0.567 %es,i,91. SKVB 0
 
Descriptive Properties
Consistence ClassClass B24 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWDE9072 / 239582

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.