MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Unreinforced, Extruded

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Water Absorption 0.010 %0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.030 %0.030 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Hardness, Rockwell R 125125ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength 93.1 MPa13500 psiASTM D638
Tensile Strength at 150°C (300°F) 3.45 MPa500 psiASTM D638
Tensile Strength at 65°C (150°F) 55.2 MPa8000 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 3.45 GPa500 ksiASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
Flexural Modulus 3.96 GPa575 ksiASTM D790
Compressive Strength 148 MPa21500 psi10% Def.; ASTM D695
Compressive Modulus 2.96 GPa430 ksiASTM D695
Shear Strength 62.1 MPa9000 psiASTM D732
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.400.40Dry vs. Steel; QTM55007
K (wear) Factor 4830 x 10-8 mm³/N-M2400 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.105 MPa-m/sec3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 21.3 kV/mm540 kV/inShort Term; ASTM D149
Dissipation Factor 0.0013
@Frequency 1e+6 Hz
0.0013
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.4 µm/m-°C
@Temperature -40.0 - 149 °C
28.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°FASTM F433
Melting Point 282 °C540 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 218 °C425 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
Canada AG NoNo
FDA YesYes
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ColorNatural
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Techtron® HPV PPS (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)

P1SM37 / 20131

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.