MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Water Absorption 0.10 %0.10 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.50 %0.50 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Hardness, Rockwell R 126126ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength 110 MPa16000 psiASTM D638
Tensile Strength at 150°C (300°F) 20.7 MPa3000 psiASTM D638
Tensile Strength at 65°C (150°F) 82.7 MPa12000 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 4.34 GPa630 ksiASTM D638
Flexural Strength 172 MPa25000 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiASTM D790
Compressive Strength 138 MPa20000 psi10% Def.; ASTM D695
Compressive Modulus 3.45 GPa500 ksiASTM D695
Shear Strength 55.2 MPa8000 psiASTM D732
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.320.32Dry vs. Steel; QTM55007
K (wear) Factor 755 x 10-8 mm³/N-M375 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.298 MPa-m/sec8500 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.9 kV/mm480 kV/inShort Term; ASTM D149
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C
@Temperature -40.0 - 149 °C
26.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.252 W/m-K1.75 BTU-in/hr-ft²-°FASTM F433
Melting Point 340 °C644 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 249 °C480 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYesNatural Only
Canada AG NoNo
FDA YesYes
NSF YesYes
USDA YesYes
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ColorsTan(Natural) or Black
Machinability51-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)
Mitsubishi Chemical Advanced Materials Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)

P1SM12A / 20089

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.