ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.1 for food contact. Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |